CZTS thin films were deposited by sol–gel spin coating method using precursor solutions prepared by dissolving copper acetate dihydrate, zinc acetate dihydrate, tin chloride and thiourea in methanol and monoethylamine then annealed in RTP furnace at 500 °C. Sol–gel precursor solutions were prepared with different Zn/Sn in a precursor solution and were annealed at different time intervals; and their effects on the optical and electrical properties of CZTS (Cu2ZnSnS4) films were investigated. The optical band-gap values were estimated to be between 1.30 and 1.88 eV while the absorption coefficients were in the range of 104 cm–1 in the visible region. The resistivity and carrier concentrations ranged from 13.12 to 2634 kΩ/□ and 1017 to 1020 cm−3, respectively. The influence of Zn/Sn ratio and annealing time on structural properties of CZTS thin films are also discussed.

Share

COinS
 
 

To view the content in your browser, please download Adobe Reader or, alternately,
you may Download the file to your hard drive.

NOTE: The latest versions of Adobe Reader do not support viewing PDF files within Firefox on Mac OS and if you are using a modern (Intel) Mac, there is no official plugin for viewing PDF files within the browser window.